Hover to Zoom
Absorption Of Fine Aggregate Test
ASTM C-AASHTO T 131-84 For determining the water absorption of fine aggregate at saturated surface dry.
Cone
Brass 40 mm, i. d at the top, a 90 mm i. d at the bottom, 75 mm height.
Tamper
Machine steel, 340 grams of weight, 25 mm dia.
Mixing Bowl
Stainless steel, round type 24 cm diameter approx.
Glass Plate
10 cm thick, 30 x 30 cm
Volumetric Flask
Heat resistance glass 500 ml ca